Rotaries  under Raw mill  cyclones Maintenance

 

  Rotaries  under R.M cyclones

1- All keys for this rotaries have a sever wear, also the key ways in the hollow shafts and motor shafts have a sever wear.

2- There is an axial movement in the in the input shaft for the gear box for the

rotary under cyclone no.2.

Rotaries  under Raw mill  cyclones
Rotaries under Raw mill cyclones

Recommendation:

 

1- Replace all keys.

2- Repair the hollow shafts and motor shafts due to the sever wear.

3- Check the bearings of the hollow shafts which have axial movement and replace the bearings if needed for rotary under cyclone no.2.

 

Action has been taken

 

1- The worn out key ways have been repaired (for motor shafts only).

2- All keys have been replaced.

3- Oil seals of high speed shafts have been changed

 

if you have any inquiry don’t hesitate to contact us [email protected]

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.