Raw mix design/calculation for more than 3 components in excel

 

 

 

 

To use the spreadsheet change the names and chemical analyses of the raw materials to whatever you want. Then enter whatever raw meal targets you want for LSF, SR and AR in column G, lines 15,16 & 17.

To solve the raw mix, click on the Data tab at the top of the excel screen and choose Solver (in the Analysis group). Then click the Solve button in the window that pops up, followed by the Okbutton in the Solver Results pop-up.

 

Download Link 

 

If you don’t know how to use Solver Function in Excel please click here 

 

click here to Download the Most Important 13 Books in Cement Industry 

click here to Download the Most Important 13 Books in Cement Industry 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.