How to Use This Calculator
- Enter oxide analysis for each raw material: check enable box to include (limestone, clay/shale, iron ore, bauxite, sandstone)
- Set target quality parameters: LSF 95-108, SM 2.0-3.0, IM 1.3-2.0
- Enter fuel data for ash absorption correction: specific heat consumption, NCV, ash content
- Click Calculate: see constrained mix proportions using all enabled materials, measured raw-meal moduli versus targets, approximate clinker chemistry, and potential Bogue compounds when within valid bounds. Unmet targets are flagged.
Raw Material Oxide Analysis (%) — Enable materials to include in mix
Material
SiO2
Al2O3
Fe2O3
CaO
MgO
Na2O
K2O
LOI
Target Parameters & Fuel Data
Target 95-108 typically
Silica Modulus (2.0-3.0)
Alumina Modulus (1.3-2.0)
Residual loss on ignition
Uncombined lime
For ash absorption calc
Net calorific value
Ash content in fuel
Coal Ash Composition (default): SiO2 | Al2O3 | Fe2O3 | CaO (%)