Cement Quarry Area Maintenance

Previous Post
Next Post

Limestone Crusher rotor &  Limestone  Crusher Belt  Maintenance

 

 

Crusher rotor
1- The bearings condition of the drive shaft is very bad.
2- There is a sever wear in the crusher rotor.
3- There is a missed lining plate in the crusher cover.
4- There is high wear in the crusher hummers.

limestone crusher rotor welding
limestone crusher rotor welding
worn out Lime stone crusher rotor
worn out Lime stone crusher rotor

 

Recommendation:

1- Replace the bearings of the drive shaft.
2- Repair the worn out rotor by welding.
3- Erect the missed lining in the crusher cover.
4- Repair the worn out hummers by welding.

Action has been taken:

1- The worn out rotor has been repaired by welding electrodes 7018.

Crusher Belt

 

The new vulcanizing connection . The drum lining not exist which cause continues drift for the rubber belt
The new vulcanizing connection . The drum lining not exist which cause continues drift for the rubber belt

1- The belt conveyor has many defected parts and cut off wires.
2- There are 2 defected vulcanizing connections.
3- There is steel cord wire separated from the middle of belt with length 400m.
4- All drums lining have a sever wear.

Recommendation:

1- Replace the belt conveyor.
2- If the belt conveyor will not be replaced completely, at least the most
defected part on the rubber belt with length 250 m should be replaced.
3- Repair all cut off parts in the middle of the rubber belt.
4- Cover the position of the separated steel wire with a vulcanizing tape.
5- Replace all worn out drums lining due to sever wear and to save the new belt
from contacting with the roller support, so it will cause.

Action has been taken

1- The most defected parts in the belt conveyor have been replaced 190 m.
2- Two cut off part has been repaired

 

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.