Sensible Heat of Solids, Liquids and Gases
The following specific heats are average values between the temperature T and the reference temperature of 20°C. So the calculation of the sensible heat difference between two temperatures is as follows:
Average Sensible Heat Cp of Solids [kJ/kg K]
Average Sensible Heat cpof Gases [kJ/Nm3K]
Average Sensible Heat cp of Fuels [kJ/kg K]
Take the next step
Your next cement plant challenge deserves more than one article. Get the complete 931-file reference library for process troubleshooting, calculations, maintenance planning and team training, including 54 ready-to-use Excel tools.
US$249.99 one-time purchase
Buy the Complete Technical Package → 931 technical files • Lifetime updates included as advertised • Pay through PayPal