Main reasons for kiln inlet spillage by ahmed el sayed

Previous Post
Next Post

Main reasons for kiln inlet spillage by ahmed el sayed

Damage in kiln inlet shelv

Damage kiln inlet scoop

Low kiln RPM with sulphate ring

Poor draught

1- ask mechanical team to keep kiln in up position to close inlet seal gap.

2- decrease kiln feed.

3- increase kiln speed.

4- maintain more kiln inlet negative pressure either by ID fan or by pass fan.

5- keep more kiln hood negative pressure.

6- focus to eliminate any ring formation or thick coating in UTZ or BZ.

7- review with quality team SO3 hot meal, clinker,LP, Mgo and SM.

8- check any build up at kiln inlet and dead corner but pay attention for team safety.

 

 

[contact-form][contact-field label=”Name” type=”name” required=”true” /][contact-field label=”Email” type=”email” required=”true” /][contact-field label=”Website” type=”url” /][contact-field label=”Message” type=”textarea” /][/contact-form]

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.