Raw mix ratios signification recommended value

Previous Post
Next Post

Raw mix ratios signification recommended value

The alumina ratio

The silica ratio

Exercise: what is the reason of a decrease of silica ratio?

LSF Lime Saturation Factor

To make clinker correctly, the raw mix must contain all the total lime (t-CaO) needed to:

o form the C4AF with the iron and one part of Al2O3

o form the C3A with the possibly remaining alumina

o form the C2S with all of the silica… then transform all of the C2S into C3S

 

Takes into account the required lime reduction

The lime saturation factor measures the little less of total lime

 

  So in practice, C real – C theoretic

Influence of C3S / C2S

Exercise: question

Exercise: answer 1

What is your diagnostic concerning third raw mix?

 

 

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.