Effects of Minor Elements11

Element Concentration Effect Raw Meal (%) TiO2 0.10 - 0.47 Flux Retards init. setting Increases strength Cr2O3 0.01 - 0.05 “Chromium Eczema” Colour Mn2O3 0.03 - 0.83 Colour

Element Concentration Effect
Raw Meal (%)
TiO2 0.10 – 0.47 Flux
Retards init. setting
Increases strength
Cr2O3 0.01 – 0.05 “Chromium Eczema”
Colour
Mn2O3 0.03 – 0.83 Colour