BALL CHARGE DESIGN

 

you will have to fill the cells which are highlighted in yellow

and the results will appear in Red

Ball charge management

 

Top up for ball wear compensation

While a Ø 90 [mm] becomes an Ø 80 [mm] an Ø 80 [mm] becomes a Ø 70 [mm] and so on …

 

 

  • The ball quantity to compensate wear (BWC) depends on the net wear (NW) and the annual cement production (ACP).
  • BWC = ACP x NW x 10^-6  [t/a]

Ball charge classification

  • Visual criteria for ball form classification (deformed/broken)

  • Standard frequency for ball charge classification

Ball charge operating cost

Download

please click here to download from mediafire 

 

 

 

Previous Post
Next Post

2 thoughts on “Confidential for Polysius Engineers – BALL CHARGE DESIGN free download excel sheet”

  1. Sir,
    I need a job for soudi cement. I already job in soudi saipem oil company.
    I am weatig you answer.

    Most respectfully.

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.