Below , I describe our exact steps for Kiln Audit & Benchmark service. If you need our service online or offline at your site please email me at [email protected]

IF YOU WORK IN A CEMENT PLANT AND YOU NEED COURSES AND MANUALS LIKE THIS MANUAL AND BOOKS AND EXCEL SHEETS AND NOTES I SPENT 23 YEARS COLLECTING THEM YOU SHOULD CLICK HERE TO DOWNLOAD THEM NOW 

Kiln Audit : What it means?

 

Review
• Present operation philosophy
• Operating parameters
• Operation / Quality targets
• Present Constraints
• Status of PID control loop operation

Establish equipment / system performance
• Production
• Heat Consumption
• Power Consumption
• Efficiency

 Benchmark
• Past performance
• Supplier guarantees
• Type of equipment / system
• Anticipated performance

Recommend for performance improvement
• Changes in operation philosophy, operating parameters, operation / quality Targets
• Modifications to individual equipment / system

Kiln Audit : Steps involved

 

Pre-audit information checklist.
• Plant base information (Flow sheet, equipment details).
• Past performance data (Run / production / reliability factor, energy consumption, quality).
• Type of fuels used and products manufactured.
• Present problems faced by plant.

Measurement / sampling tools
• Instruments (availability, suitability, functioning, calibration)

Measurement / sampling plan
• Measurements / sampling / analysis requirments with priority level.
• Frequency of measurement / sampling.

Calculation tools
Data from other plant audits
Result Interpretations.
Report writing
Reference documents

Kiln Audit : Pre-audit information

 

The Plant
• Location (place, nearest city, MSL, Ambient temperatures, % RH)
• Local line No. (if any)
• Supplier
• Year supplied
• Supplier guarantees (Production, heat consumption, power consumption etc).

Preheater & Pre-Calciner
• No. of stages
• No. of strings
• Whether In line calciner / separate calciner / AS / AT
• Type of calciner: Low NOx / hot point etc.
• Cyclone sizes
• Calciner dimensions with sketch (showing firing / feed /Tertiary air entry point locations)
• Feeding arrangement (air lift / bucket elevator)

Kiln
• Size (Diameter x Length)
• No. of supports (2 / 3)
• Slope (3.5 / 4%)
• Maximum speed, rpm
• Lining thickness, mm
• Installed motor power

Cooler
• Supplier
• Supplier product code (e.g. FLS COOLAX 1284)
• Type (Conventional chamber aerated / Beam aeration etc.)
• Type of inlet (e.g. Fixed)
• No. of Grates
• Dimensions (width x Length)
• Effective Grate area
• No. of compartments
• No. of fans (Specify v-belt / direct drive, variable / fixed speed)
• Enclose sketch showing grate plate layout with aeration arrangement
• Vent air de-dusting arrangement (ESP, Heat exchanger + Bag filter)
• Emergency cooling arrangements (fresh air / water spray)
• Cooling air & Vent air fan specifications
• Tertiary air take-off point (through kiln hood / separate)
• Dust Settling Chamber in tertiary air line?
• Any hot air tapping (for raw / coal / cement mill)
• Under-grate dust collection arrangement (drag chain / hoppers with pneumatic gates)

Burner
• Supplier
• Supplier product code (e.g. FLS Duoflex)
• Type (Uni-flow / Multi-channel?)

Miscellaneous
• Fuels used (with proportions, way of preparation)
• Sketch showing gas & material flows
• Present performance (Production, heat / power consumption)
• Present constraints
• Sketch indicating measurement / sampling point locations
• Modifications done w.r.t. original supply (e.g. changed to Lafarge Burner, installation of Hurrivanes in preheater cyclone)

Kiln Audit : Samples & analysis

 

Inputs

Kiln Feed
• Fineness (Residues on 90 and 212µ)
• Temperature
• Moisture
• Uniformity (KFUI),
• Homogenization (Standard deviation of CaO/CaCO3/RC3S at silo exit)
• Burnability (K1450)
• Coarse quartz and calcite content
• LOI
• Chemical analysis (incl. minor oxides and chlorine)
• Organic carbon
• Water of crystallization / hydration
• Sulfur as pyrites
• TC

Fuel, as fired
• Moisture
• Fineness (Residues on 90 and 212µ)
• Temperature
• Heat value
• Proximate analysis
• Ultimate analysis

Outputs

Clinker
• Temperature
• Sieve analysis
• Free lime
• Liter weight
• LOI
• Chemical analysis (incl. Minor oxides)
• Microscopy

Dust from Preheater
• PSD
• LOI
• Chemical analysis (incl. Minor oxides)

With in Process

Bottom stage exit material
• LOI
• Temperature
• Chemical analysis (incl. minor oxides)
• Un-burnt Carbon

Kiln Audit : Sampling frequency

Kiln Audit : Field Measurements

 

 Preheater

Preheater Exit Gas (Downcomer duct)
• Temperature
• Static Pressure
• Flow
• Gas analysis (O2, CO, CO2, SO2, NOx)
• Dust concentration

Calciner exit
• Temperature
• Static Pressure
• Gas analysis (O2, CO, CO2, SO2, NOx)

Each cyclone inlet and outlet
• Temperature
• Static pressure
• Gas analysis (O2, CO, CO2)

Kiln

Kiln inlet
• Temperature
• Static Pressure
• Gas analysis (O2, CO, CO2, SO2, NOx)

Primary Air (Kiln / Calciner Burner)
• Flow
• Pressure
• Temperature

Transport air for fuel
• Flow
• Temperature

Cooler

Cooling air
• Flow
• Temperature
• Pressure (at fan outlet, for each individual duct after flap damper)

Cooler vent air
• Temperature
• Static pressure
• Flow

Secondary air
• Temperature

Kiln hood
• Pressure

Tertiary air (at cooler end)
• Temperature
• Static pressure
• Flow (if possible)

Kiln Audit : Other Measurements

 

Mass flows
• Kiln Feed
• Clinker (by drop test)
• Preheater exit dust (by drop test)
• Fuel to Kiln
• Fuel to calciner

Power
• Kiln main drive
• Preheater fan
• Cooler vent fan
• Individual cooling air fan
• Total shop

Surface temperatures
• Kiln shell
• All components of preheater (cyclones incl. risers, material pipes, smoke chamber, kiln riser pipe, calciner vessel)
• Tertiary air duct
• Kiln hood
• Cooler walls

Kiln Audit : Measurements

 

Remember!
• To cross-check CCR indications w.r.t. field measurements
• To have Minimum 2 sets of measurements
• To perform measurements during stable kiln operation
• To Specify measurement point locations
• To check suitability of flow measurement point (8D – 3D criteria)
To record:
• Pitot tube constants
• Duct diameters at flow measurement point
• Emissivity used for surface temperature measurement
• Surface areas required for radiation loss calculation
• Transport air details (fuel / feed)

Kiln Audit : Measurement tools

• Gas analyzer (2 Nos.) : With CO, CO2, O2, NOx, SO2 sensor

• Digital manometer (1 each)
Low range: 0–100 mmWG for Pd measurement
High range: 0–4000 mmWG

• Thermocouple with indicator (2 Nos.)
• Radiation pyrometer (1 No.)
• Stroboscope / Taco meter (1 No.)
• Measuring tape (2 Nos.)
• Insulated container for clinker temperature measurement (1 No.)

• Pitot tubes
S type, 2m long (2 Nos.)
L type for primary air flow measurement (1 No.)

Kiln Audit : Operating parameters

• Kiln Speed
• Preheater fan speed & damper opening
• Tertiary air duct damper position
• Cooler grate speeds
• Cooler under-grate pressure (way of calculation)
• Ratios used for grate-2, 3 speed w.r.t. grate-1 speed
• Individual cooler fan speed, damper opening
• Cooler vent fan speed, damper opening
• If SLC kiln, feed dividing gate (at PH Top) position
• Material dividing gate position for material diverted to kiln riser
• Primary air fan speed, damper opening
• Any other relevant parameter

Kiln Audit : Miscellaneous

• Check performance of PID control loops
• Check adequacy Sampling / measurement frequency from quality /operation / process aspects
• Look for sources of air leakages / false air entry in to the system
• Understand present constraints in terms of operation / quality
• Analyze Stoppages / Slow downs
• Monitor safety
• Record fuel and power cost

Kiln Audit : Calculation tools

 

Pitot Measurement
• For gas / air flow calculation

Air Distribution
• Compare cooler flows w.r.t. recommended

Cooler Heat Balance
• K – factor
• Recovery ratio
• Cooling efficiency
• Cooler loss

Kiln Shell & Preheater losses
• For calculation of surface / radiation heat loss

Heat & Mass Balance for Kiln
• Overall heat balance of pyro-processing section

Kiln Audit : Benchmarking

 

Above , I describe our exact steps for Kiln Audit & Benchmark service. If you need our service online or offline at your site please email me at [email protected]

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.