optimize CGB to fit Ball Mill, we applied technical modification as followings:

Previous Post
Next Post

Contents

Ball Mill optimize

 

 

Attention!! to Download Most Important Books in Cement industry reviewed from more than two thousands people + Manuals and noted from big Cement Companies like F L  S , Holcim Lafarge , Cemex , + Excel sheets for calculations process Click here Now 

 

In order to optimize our CGB to fit Ball Mill, we applied technical modification as followings:

1)The length of 1st Chamber is extended

2)The diaphragm is exchanged.

3)An air-clink separator is installed to the end of the mill,and exchange of the outlet diaphragm.

4)Technical modification is performed on activation rings.

5)Rejection rate of Separator is adjusted.

6)Adjust the HC-steel balls loading rate in 1st chamber.

7)Exchange lower loading amount of HC-steel balls into ceramic grinding balls in 2nd chamber.

 

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.

Ask a Cement Engineer ×
Hello! Ask me any cement plant technical question — kiln, grinding, quality, maintenance, preheater. I'll give you a practical answer.