Effects of Environmentally Relevant Compounds

Compound Concentr. Effect Raw Meal Pyritic Sulfur 0 - 0.8 % Emissions (10-20% - SO2) Organic Carbon 0.05 - 0.7 % Emissions (1-10 % - Volatile Org. Carbon) Ammonium 20-500 ppm Emissions - Ammoniac - Aerosol (NH4Cl, NH4NO3, …) - NOx

Compound Concentr. Effect
Raw Meal
Pyritic Sulfur 0 – 0.8 % Emissions
(10-20% – SO2)
Organic Carbon 0.05 – 0.7 % Emissions
(1-10 % – Volatile
Org. Carbon)
Ammonium 20-500 ppm Emissions
– Ammoniac
– Aerosol (NH4Cl, NH4NO3, …)
– NOx