Jaya jyothi cement coal Mill bag filter fire

Previous Post
Next Post

3 thoughts on “Jaya jyothi cement coal Mill bag filter fire”

  1. Do not allow bag filter temp not more then75 C.purg inert or Co2 gas when mill is stopped for a longer period.specially when usage of high volatile coal.
    In case of pet coke there is rare possibility of fire.