Preparation & Handling of Alternative Fuels (AF)

Previous Post
Next Post

Preparation & Handling of Alternative Fuels (AF)

Waste for Cement Kiln Firing – Examples

 

Alternative Fuel Preparation – Why?

  • Alternative fuel preparation is required to change the waste’s physical properties.

-Granulometry (Size)

-Water Content

-Foreign Bodies

-Viscosity

  • A homogeneous alternative fuel allows a higher substitution rate.

Alternative Fuel Preparation – How?

Solid Waste – Example Waste Tyres

 

Solid Waste – Cost of Shredding

Solid Alternative Fuel Installation – General Flowsheet

Size Classification of Solid AFs

Storage & Extraction of Alternative Fuels

Storage & Extraction – Fine Solids

Storage & Extraction – Lump Fuel

Pneumatic Kiln Feeding

Guidelines

-Separation of oversizes & metals

-Introduction to pneumatic transport through a rotary valve

-Pneumatic transport as short and straight as possible.

-Injection through a pipe, parallel and on top of the main burner, or a central channel if available.

Gravimetric Kiln Feeding

  • Actuated double or tripple pendulum flap gate

 

  • Actuated shut-off gate(s)

-Protection of AFR feeding system during upset kiln operation.

-De-coupling of AFR feeding system.

Liquid AF Installation – General Flowsheet

Filtering

  • Discharge filter is mandatory
    (for pump protection and to avoid atomizer blockage)
  • Standard solution: Double basket filter (manual cleaning)
  • Screen size depends on fuel specification:
    Recommended 1.5 mm, max. 5 mm (for good atomization)

Storage & Mixing of Alternative Fuel in Cement industry

  • Minimum 2 tanks (one for kiln feed, one for new deliveries)
  • Vertical installation
  • Conical or rounded bottom
  • Continuous mixing with mechanical agitator (circulating flow only second choice)
  • Retention wall
  • Fire protection (water and foam)

Kiln Feeding Pumps for Liquid AF

  • 2 Pumps in parallel (one stand by)
  • Spec.: Particles (wear), continuous flow (no pulsations) and high pressure
  • Standard pumps for liquid AF:

Screw Pole Pump

-little pulsations

-not suited for very abrasive solids and solvents

Membrane Pump

-large pulsations

-suited for solvents

Flow Measurement & Injection

Coriolis Type Flow Meter

  • no wear parts, no flow restrictions
  • simultaneous measurement:

-flow rate [m3/h]

-Density [kg/m3]-  correlation to water content

-Temperature [°C]

Two-phase Nozzle

  • atomization with pressurized air or steam
  • design of atomizer depends on max. particle size

 

for more information please contact us 

 

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.