To download the below and all other Useful Books and calculations Excel sheets please click here
To download the below and all other Useful Books and calculations Excel sheets please click here
Miscellaneous Formulas
Ideal Gas Conversion
The formula below is used to convert volumes of ideal gases from normal conditions (0°C, 1’013 mbar) to the volumes Vactat actual gas conditions (T, p) in the process.

Barometric Pressure
The average barometric pressure p at a plant altitude (above sea level) can be calculated using the following approximation formula.

Air Inleakage through Holes and Apertures
Air leakage through apertures (e.g. kiln inlet seal, kiln hood) can be calculated with the Bernoulli equation:

For ambient conditions of around 20°C and 1 bar (air density of 1.19 kg/m3) theabove formula can be simplified as:

for More information
Excellent ,very informative …Merry Xmass
very useful