Kiln/Cooler Calculation Formulas

 

Material Residence Time in Kiln

The retention time of the material in a dry rotary kiln can be determined with the
formula from Duda Cement Data Book:

Material Filling Degree in Kiln

Clinker Cooler Exit Temperature

The achievable clinker temperature at the cooler exit with a given cooling air volume VAir can be calculated as (Rule of Thumb):

Transport Efficiency of Grate Cooler

Reference

Holcim 

 

Previous Post
Next Post

2 thoughts on “Kiln/Cooler Calculation Formulas”

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.