Bogue formula

Previous Post
Next Post

Bogue formula

Clinker minerals

Decarbonated kiln raw mix

Any changes in the 4 raw mix elements will change the proportions of the 4 clinker minerals, and thus the clinker quality

The type of clinker required determines what the proportions of the 4 minerals should be

Exercise