Effect of Minor Elements on Clinker and Cement by Javed I. Bhatty

Effect of Minor Elements on Clinker and Cement by Javed I. Bhatty Senior Scientist, CTLGroup, 5400 Old Orchard Road, Skokie, Illinois 60077 847.972.3082, jbhatty@ctlgroup.com   The effect of minor elements on the production and performance of portland cement have been presented in this report. The elements studied are lead, molybdenum, antimony, copper, cadmium, beryllium, titanium, …