-Shell Liner Thickness Ball Charge Remarks – sizes, shape, contamination, breakages

-Shell Liner Lifter Thickness Ball Coating Remarks

-Shell Liner Remarks – crack, gaps…. Ball Classification Remarks

-Inlet Head Liner Thickness Discharge Grate Slot Size-Average

-Inlet Head Liner Remarks Discharge Grate Slot Size-Maximum

-Inlet Opening Remarks Discharge Grate Metal Thickness – gaps etc.

-Height Liner, to Balls – Average

-Discharge Grate Percent Blinded

-Width Across Balls – Average

-Discharge/Centre Screen Percent Blinded

-Calculated Percent Fill – mill ran out Height of Material relative to media

-Build up on water injection lance Calculated Percent Fill

– mill crash stopped

-Presence of material nibs

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.