Kiln & Pre-Heater Essential figures and there Reference for Bench marking

Previous Post
Next Post

Kiln & Pre-Heater Essential figures and there Reference for Bench marking

S.NO Parameters Unit Norms
1. Specific thermal loading (max) G cal/h/m
4.0 – 5.0
2. Specific volumetric loading (Sustainable) tpd/ m
4.5 – 6.5
3. Specific volumetric loading (Peak) tpd/ m
7.0
4. Percentage filling % 13 – 17
5. Retention time (Minimum)
➢ In Line calciner
➢ Separate Line calciner
➢ Caciner with Pet coke firing
6. Tertiary air temperature

Sec.
o
3
3
C
850 – 1000
7. Secondary air temperature
C
1000 – 1200
8. Burner flame momentum, For normal coal % m/s 1400 – 1600
9. Burner flame momentum, For Pet coke % m/s 1800 – 2200
10. Margin in Burner capacity % 25
o
2

3.2
2.6
4.5

Previous Post
Next Post

2 thoughts on “Kiln & Pre-Heater Essential figures and there Reference for Bench marking”

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.