2018 Target Days of Storage in Cement industry

Previous Post
Next Post

2018 Target Days of Storage in Cement industry

S.No Item / Equipment Days for storages
1.
Limestone Storage/
Preblending Stockpile*
Chapter – III
Operating Hours
Chapter – IV
Days of Storage

7
2. Raw Meal Storage (Active) 1 – 1.5
3. Clinker 7-15
4. Cement 3-10
5. Fuel Storage* 15-30 (depending upon lead time)
6. Additive / corrective * 15-30 (depending upon lead time)
7. Slag 7 – 15 (depending upon lead time)
8. Fly ash 3 – 7 (depending upon lead time)
* Capacity calculated should be inclusive of moisture content and handling
loss (2%)

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.