Kiln Shell Ovality measurement (Shelltest)
Procedure

 

PURPOSE

The kiln shell ovality measurement (also known as Shelltest) measures the elastic  deformation on the areas adjacent to the tires. An excessive ovality value will have a negative impact on the lifetime of the refractory bricks and must be kept under acceptable limits (which vary according to kiln diameter). The creep (relative movement must be measured as well, since they are closely related and it is the shimming (reduction of clearance between tire and shell) the method to reduce ovality.

As can be inferred, this measurement is relevant for kilns with loose (floating) tires. Those equipped with the more modern splined (toothed) tires are not  affected; there is virtually no creep and therefore the ovality measurement is not required .

HGRS recommends the measuring device “Shelltest” which is briefly described in this paper. Nowadays, several suppliers (e.g. Refratechnik, Phillips Kiln Services) offer an electronic version of this device, in case a plant or Group Company needs to buy a new one.

 

Download link 

Previous Post
Next Post

3 thoughts on “Kiln Shell Ovality measurement (Shelltest) Procedure”

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.