How to Use This Calculator
- Enter raw meal loss on ignition: LOI % from chemical analysis
- Enter process losses: preheater dust loss %, dust LOI, bypass dust if applicable
- Enter fuel ash incorporated: ash actually retained in clinker as a percentage of dry kiln feed (not coal ash percentage alone)
- Click Calculate: to see estimated clinker yield, dry kiln-feed-to-clinker factor, net dust solid losses and fuel ash contribution
Raw Meal & Process Losses
Loss on ignition; typical 34–37%
% of dry kiln feed permanently lost as dust; exclude returned dust and bypass dust
LOI of the net dust discharged from the system; not recirculated dust
Actual fuel ash retained in clinker per tonne dry kiln feed; 0 if unavailable
% of dry feed exiting the system via bypass; do not include in preheater dust input
LOI of bypass dust if applicable