Contents
Practical Guide: Clearing Blockages in Limestone Crusher in Cement Plant
![]()
TO Download this post and all the books and excel sheets and my personal notes and presentations I collected about cement industry in the last 30 years click the below paypal link
Introduction
Clearing blockages in the limestone crusher is essential for maintaining uninterrupted production in cement plants. This practical guide provides step-by-step instructions for clearing blockages safely and efficiently. Additionally, it highlights popular raw crushers used in cement industries, their models, expected costs, and relevant references.
1. Importance of Clearing Blockages
Blockages in the limestone crusher can lead to downtime, reduced production capacity, and potential equipment damage. Clearing blockages promptly ensures continuous operation and prevents costly disruptions.
2. Steps to Clear Blockages
a. Safety Precautions:
- Before starting any maintenance work, ensure the crusher is shut down, and all power sources are isolated.
- Wear appropriate personal protective equipment (PPE), including gloves, safety goggles, and hearing protection.
b. Identify Blockage Location:
- Conduct a visual inspection to locate the blockage within the crusher chamber.
- Use a flashlight or inspection camera if visibility is limited.
c. Remove Obstructions:
- If the blockage is caused by oversized or irregularly shaped material, manually remove it using a pry bar or rock hammer.
- Use caution to avoid injury and damage to crusher components.
d. Clear Buildup or Congestion:
- If the blockage is due to material buildup or congestion, use a long-handled scraper or wire brush to dislodge the material.
- Work methodically and systematically to clear the entire crusher chamber.
e. Check Crusher Operation:
- After clearing the blockage, visually inspect the crusher components for signs of damage or wear.
- Start the crusher and run a test cycle to ensure smooth operation and proper clearance of material.
3. Popular Raw Crushers in Cement Industries
a. Jaw Crushers:
- Models: Sandvik CJ Series, Metso Nordberg C Series, Terex Finlay J Series.
- Expected Cost: $50,000 – $500,000 USD (depending on capacity and features).
b. Impact Crushers:
- Models: Sandvik QI Series, Hazemag AP Series, Metso Nordberg NP Series.
- Expected Cost: $80,000 – $1,000,000 USD (depending on capacity and features).
c. Cone Crushers:
- Models: Metso Nordberg HP Series, Sandvik CH Series, Terex Cedarapids MVP Series.
- Expected Cost: $100,000 – $1,500,000 USD (depending on capacity and features).
4. References
- Cement Manufacturer’s Association (CMA) Guidelines for Crusher Maintenance in Cement Plants.
- Occupational Safety and Health Administration (OSHA) Guidelines for Working Safely with Crushers.
- Equipment Manufacturers’ Manuals and Technical Specifications.
Conclusion
Clearing blockages in the limestone crusher is a critical maintenance task in cement plants to ensure uninterrupted production and prevent equipment damage. By following the steps outlined in this guide and using popular raw crushers, cement manufacturers can maintain efficient operations and minimize downtime.