Optimum sulphate content

Previous Post
Next Post

Optimum sulphate content

–Why?

o to obtain a good workability

o silicates normal hydration

o better strength

–The optimal quantity of sulphates depends on

o % C3A & C4AF

o cement fineness

o sulphates reactivity

Sulphates

 

Optimum sulphate content  Low alkaline sulphates level

Optimum sulphate content High alkaline sulphates level

 

Sulphates  Action on hydration

Sulphates

o blocking ettringite

Alkaline sulphates

o accelerators

setting time (sometimes a little bit shorter)

higher initial strengths

lower 28 days strengths

o maintains high pH

protects reinforcement

but Ca++ lower

favorable effect on shrinkage

in plastic phase

in hardened phase

o reduces expansion

Sulphates Action on hydration

Alkaline sulphates

o favorable action in steam curing (increase strength)

o increase cement agglomeration

syngenite – gorgeyite

o alcali-aggregate reaction

o reaction with organic materials

stone staining

concrete staining…

efflorescences

Sulphates

Anhydrous sulphates of clinker

o  Arcanite  K2SO4

oLangbeinite  2 Ca SO4, K2SO4

o Aphtitalite  Na2SO4, K2SO4

Hydrated sulphates

o Syngenite  Ca SO4, K2SO4 , H2O

o Gorgeyite  5 Ca SO4, K2SO4 , H2O

Sulphates Compared solubility of some sulphates

 

 

Previous Post
Next Post

Leave a Comment

Your email address will not be published. Required fields are marked *

10 Essential Cement Plant Calculations

Free PDF — clinker chemistry, kiln sizing, ball mill power, and more. Enter your email and we'll send it immediately.

No spam. Unsubscribe anytime.

Check Your Inbox

Your PDF is on its way. Plus 6 more emails with cement plant tips and case studies.