Figure 9.1.8. In the autoclave expansion test for soundness, 25 mm square bars are exposed to high temperature and pressure to determine the volume stability of the cement paste. (23894)

Figure 9.1.8. In the autoclave expansion test for soundness, 25 mm square bars are exposed to high temperature and pressure to determine the volume stability of the cement paste. (23894)

Figure 9.1.8. In the autoclave expansion test for soundness, 25 mm square bars are exposed to high temperature and pressure to determine the volume stability of the cement paste. (23894)